Polymer Property : Tensile Stress = 1.48 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 1.48 MPa

@Strain 100 %
215 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® A9850 TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
Tensile Stress 1.48 MPa

@Strain 100 %
215 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® C4640 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Stress 1.48 MPa

@Strain 100 %
215 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P3950CT TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 1.48 MPa

@Strain 100 %,
Temperature 23.0 °C
215 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynalloy™ OBC 8100-N50 Thermoplastic Elastomer (TPE)
Dynalloy™ OBC8100-N50 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t..
Tensile Stress 1.48 MPa

@Strain 50.0 %
214 psi

@Strain 50.0 %
Average; ASTM D412 Method A
Seals Eastern 5722A Fluorocarbon-Elastomer
Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Exce..
Tensile Stress 1.48 MPa

@Strain 300 %
215 psi

@Strain 300 %
ASTM D412
Teknor Apex Telcar® TL-2635C Thermoplastic Elastomer
Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi..
Tensile Stress 1.48 MPa

@Strain 300 %
215 psi

@Strain 300 %
ASTM D412
Teknor Apex Telcar® TL-2635D Thermoplastic Elastomer
Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi..
Tensile Stress 1.48 MPa

@Strain 0.000 %,
Temperature 120 °C
215 psi

@Strain 0.000 %,
Temperature 248 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon  (Unverified Data**)
Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood..
Tensile Stress 1.48 MPa

@Strain 0.200 %,
Temperature 40.0 °C
215 psi

@Strain 0.200 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610  (Unverified Data**)
Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie..