Mechanical Properties Metric English Comments
Tensile Stress 1.45 MPa

@Strain 300 %
210 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® A9930 TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
Tensile Stress 1.45 MPa

@Strain 100 %,
Temperature 23.0 °C
210 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ 9555-1 Thermoplastic Elastomer (TPE)
Versaflex™ 9555-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to ..
Tensile Stress 1.45 MPa

@Strain 100 %,
Temperature 23.0 °C
210 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ 9555-9 Thermoplastic Elastomer (TPE)
Versaflex™ 9555-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to ..
Tensile Stress 1.45 MPa

@Strain 100 %,
Temperature 23.0 °C
210 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ OM 9-801N Thermoplastic Elastomer (TPE)
Versaflex™ OM 9-801N is designed for overmolding onto a wide variety of substrates including PC, ABS, PC/ABS, HIPS, PPO, acetal, acrylic and copolyester. - Bonds to a Variety Of Substrates - Rubber..
Tensile Stress 1.45 MPa

@Strain 100 %,
Temperature 21.0 °C
210 psi

@Strain 100 %,
Temperature 69.8 °F
Die C2 hr; ASTM D412
PolyOne Versalloy™ XL 9055-1 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9055-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov..
Tensile Stress 1.45 MPa

@Strain 100 %,
Temperature 23.0 °C
210 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versalloy™ XL 9055X-9 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9055X-9 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Overmold Adhesion to Polypro..
Tensile Stress 1.45 MPa

@Strain 300 %
210 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P1740 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 1.45 MPa

@Strain 300 %
210 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P2635 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 1.45 MPa

@Strain 300 %
210 psi

@Strain 300 %
ASTM D412
Teknor Apex Telcar® TL-2635A Thermoplastic Elastomer
Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi..
Tensile Stress 1.45 MPa

@Strain 300 %
210 psi

@Strain 300 %
ASTM D412
Teknor Apex Telcar® TL-2635B Thermoplastic Elastomer
Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi..
Tensile Stress 1.45 MPa

@Strain 300 %
210 psi

@Strain 300 %
ASTM D412
Teknor Apex Telcar® TL-97-T0214B-55 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Stress 1.45 MPa

@Strain 97.65 %,
Temperature 120 °C
210 psi

@Strain 97.65 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b..
Tensile Stress 1.45 MPa

@Strain 112.5 %,
Temperature 120 °C
210 psi

@Strain 112.5 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b..
Tensile Stress 1.45 MPa

@Strain 0.000 %,
Temperature 0.000 °C
210 psi

@Strain 0.000 %,
Temperature 32.0 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66  (Unverified Data**)
Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in..
Tensile Stress 1.45 MPa

@Strain 97.65 %,
Temperature 120 °C
210 psi

@Strain 97.65 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 1.45 MPa

@Strain 112.5 %,
Temperature 120 °C
210 psi

@Strain 112.5 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved