Polymer Property : Tensile Stress = 0.480 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 0.480 MPa

@Strain 0.260 %,
Temperature 150 °C
69.6 psi

@Strain 0.260 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610  (Unverified Data**)
Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by..
Tensile Stress 0.480 MPa

@Strain 0.0200 %,
Temperature -40.0 °C
69.6 psi

@Strain 0.0200 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1000 BK385 Nylon 1010
UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight...
Tensile Stress 0.480 MPa

@Strain 0.0200 %,
Temperature -20.0 °C
69.6 psi

@Strain 0.0200 %,
Temperature -4.00 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET  (Unverified Data**)
65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers
Tensile Stress 0.480 MPa

@Strain 0.140 %,
Temperature 0.000 °C
69.6 psi

@Strain 0.140 %,
Temperature 32.0 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers