Polymer Property : Modulus of Elasticity = 2000 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 13.8 GPa

@Thickness 1.57 mm
2000 ksi

@Thickness 0.0620 in
LW; ASTM D229
Industrial Laminates/Norplex NP509 Glass Fabric
Description: Woven glass fabric, melamine resin laminate. Very hard, flame resistant, machining grade with excellent electrical properties in high humidity conditions. High physical strength and exc..