Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 13.8 GPa @Thickness 1.57 mm |
2000 ksi @Thickness 0.0620 in |
LW; ASTM D229 |
Industrial Laminates/Norplex NP509 Glass Fabric Description: Woven glass fabric, melamine resin laminate. Very hard, flame resistant, machining grade with excellent electrical properties in high humidity conditions. High physical strength and exc.. |