Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.21 J/cm @Temperature -51.1 °C |
13.5 ft-lb/in @Temperature -60.0 °F |
ASTM D256 |
PlastiComp Complet® LGF60-PA66 MT 60% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Izod Impact, Notched | 7.21 J/cm @Temperature -30.0 °C |
13.5 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXD1414T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was suppli.. |
|||
Izod Impact, Notched | 7.21 J/cm @Thickness 6.35 mm, Temperature 0.000 °C |
13.5 ft-lb/in @Thickness 0.250 in, Temperature 32.0 °F |
ASTM D-256 |
Axiall 7801 Rigid PVC, Extrusion, White, High Impact Profile Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 7.21 J/cm @Thickness 6.35 mm, Temperature 0.000 °C |
13.5 ft-lb/in @Thickness 0.250 in, Temperature 32.0 °F |
ASTM D-256 |
Axiall 7803 Rigid PVC, Extrusion High Impact Profile Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 7.21 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
13.5 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D-256 |
Axiall SP-6235 Rigid PVC, Molding Georgia Gulf SP-6235 is a high flow rigid PVC compound designed for electrical and custom molding applications. This compound features excellent physical properties, high melt flow and exceptionall.. |