PlastiComp Complet® LGF60-PA66 MT 60% Long Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 60% Glass Fiber Filled
Manufacturer PlastiComp
Trade Name Complēt®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Complet® LGF60-PA66 MT 60% Long Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.70 g/cc
1.70 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 268 MPa
38900 psi
ASTM D638
Elongation at Break 2.0 - 3.0 %
2.0 - 3.0 %
ASTM D638
Tensile Modulus 16.9 GPa
2450 ksi
ASTM D638
Flexural Strength 372 MPa
54000 psi
ASTM D790
Flexural Modulus 15.59 GPa
2261 ksi
ASTM D790
Izod Impact, Notched 7.00 J/cm

@Temperature 22.2 °C
13.1 ft-lb/in

@Temperature 72.0 °F
ASTM D256
7.21 J/cm

@Temperature -51.1 °C
13.5 ft-lb/in

@Temperature -60.0 °F
ASTM D256
Izod Impact, Unnotched 17.78 J/cm
33.31 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 246 °C
475 °F