Mechanical Properties Metric English Comments
Izod Impact, Notched 3.47 J/cm

@Temperature -30.0 °C
6.50 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer (Europe-Africa-Middle East)
PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp..
Izod Impact, Notched 3.47 J/cm

@Thickness 3.17 mm
6.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
PTS Trilac® ABS-HS6500 High Impact ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched 3.47 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
6.50 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM-D256
Ineos ABS Lustran® 633 ABS, Injection Molding Grade
Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical ..
Izod Impact, Notched 3.47 J/cm

@Temperature -29.0 °C
6.50 ft-lb/in

@Temperature -20.2 °F
3.2 mm (0.125 in) notch
Kraton® G1654 + PPE blend (20/80)
Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PPE significantly improves the..
Izod Impact, Notched 3.47 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
6.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Diamond Polymers Centrex® 833 Sheet Extrusion Grade
Centrex 833 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it ..