Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.48 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
8.40 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8004 UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV Resistance and High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 4.48 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
8.40 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8004 UV MB Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV Resistance and High Heat ResistanceTPCI# 6816121Information provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 4.48 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
8.40 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8012 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 4.48 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
8.40 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8004 Availability: North AmericaForms: PelletsFeatures: General Purpose and High Impact ResistanceInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 4.48 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
8.40 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS FR IM Availability: North AmericaForms: PelletsFeatures: Flame Retardant and High Impact ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 4.48 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
8.40 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS IM Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 4.48 J/cm @Temperature 23.0 °C |
8.39 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Tenite 485E3720023 Butyrate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Izod Impact, Notched | 4.48 J/cm @Thickness 3.17 mm, Temperature -22.0 °C |
8.39 ft-lb/in @Thickness 0.125 in, Temperature -7.60 °F |
ASTM D256 |
Diamond Polymers DIAMALOY 1418EF Polycarbonate/Polyester Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |