Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.48 J/cm @Temperature 23.0 °C |
8.39 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Tenite 485E3720023 Butyrate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Izod Impact, Notched | 4.48 J/cm @Thickness 3.17 mm, Temperature -22.0 °C |
8.39 ft-lb/in @Thickness 0.125 in, Temperature -7.60 °F |
ASTM D256 |
Diamond Polymers DIAMALOY 1418EF Polycarbonate/Polyester Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |