Polymer Property : Izod Impact, Notched = 4.22 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.26 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
4.22 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical AF312A ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
Izod Impact, Notched 2.26 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
4.22 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical AF312T ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
Izod Impact, Notched 2.26 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.22 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical HI121H ABS, High Stiffness
Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 2.26 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
4.22 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LG713 ABS, Low Gloss
Feature: Extrusion Molding, Low Gloss, ExtrusionApplication: Automotive Interior Housing (Cover Etc)CAS No. 25120-20-1, 9003-56-9 and 31621-07-5Information provided by LG Chemical
Izod Impact, Notched 2.26 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.22 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical SG175 ABS, Super Surface Gloss
Feature: Injection Molding, Super Surface GlossApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 2.26 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
4.22 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical TR552 MABS, Transparency, High Impact, Chemical Resistance
Feature: Injection Molding, Transparency, High Impact, Chemical ResistanceApplication: Electric/Electronic Applications, Copier, Printer etcCAS No. 9011-14–7 and 9003-56-9Information provided b..
Izod Impact, Notched 2.26 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.22 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical TR552 MABS, Transparency, High Impact, Chemical Resistance
Feature: Injection Molding, Transparency, High Impact, Chemical ResistanceApplication: Electric/Electronic Applications, Copier, Printer etcCAS No. 9011-14–7 and 9003-56-9Information provided b..
Izod Impact, Notched 2.26 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.22 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical XR401 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (lamp housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 ..
Izod Impact, Notched 2.26 J/cm

@Thickness 6.35 mm
4.22 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® LX-0987EXS ABS, Unreinforced Metallic-Look
Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.26 J/cm

@Thickness 6.35 mm
4.22 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® SR-0305 ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.26 J/cm

@Thickness 6.35 mm
4.22 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® LX-0987EXS ABS, Unreinforced Metallic-Look
Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.26 J/cm

@Thickness 6.35 mm
4.22 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® SR-0305 ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.26 J/cm

@Temperature 23.0 °C
4.22 ft-lb/in

@Temperature 73.4 °F
ASTM D256
SCG Chemicals EL-Leneâ„¢ H5211P High Density Polyethylene Pipe Resin
Key Characteristics: Good processing, high thermal stabilityRecommended Applications: Water pipes, conduit, sewage drainage pipesInformation provided by SCG Chemicals
Izod Impact, Notched 2.26 J/cm

@Thickness 3.20 mm
4.22 ft-lb/in

@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron AN450N Flame Retardant ABS
Flame Retardant- V0 at 2.0mmInformation provided by Bhansali
Izod Impact, Notched 2.26 J/cm

@Thickness 3.20 mm
4.22 ft-lb/in

@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron IM14GL ABS Injection Molding Grade
Super High Rigidity, Medium Impact, High Chemical ResistanceInformation provided by Bhansali
Izod Impact, Notched 2.26 J/cm

@Thickness 6.40 mm
4.22 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron TG3MM ABS Injection Molding Grade
Medium Flow, Medium Impact, high RigidityInformation provided by Bhansali
Izod Impact, Notched 2.25 J/cm

@Thickness 3.20 mm
4.22 ft-lb/in

@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron SE-22 FR Flame Retardant ABS Grade
Information provided by Bhansali
Izod Impact, Notched 2.26 J/cm

@Thickness 6.40 mm
4.22 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron TG3MM ABS Injection Molding Grade
Medium Flow, Medium Impact, high RigidityInformation provided by Bhansali
Izod Impact, Notched 2.26 J/cm

@Thickness 3.20 mm
4.22 ft-lb/in

@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron IM21G ABS Injection Molding Grade
Super High Gloss, Medium ImpactInformation provided by Bhansali
Izod Impact, Notched 2.25 J/cm

@Thickness 3.20 mm
4.22 ft-lb/in

@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron SE-22 FR Flame Retardant ABS Grade
Information provided by Bhansali
Izod Impact, Notched 2.26 J/cm

@Thickness 3.20 mm
4.22 ft-lb/in

@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron AN450N Flame Retardant ABS
Flame Retardant- V0 at 2.0mmInformation provided by Bhansali
Izod Impact, Notched 2.26 J/cm

@Thickness 3.20 mm
4.22 ft-lb/in

@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron KU600N ABS Heat Resistant
High ImpactInformation provided by Bhansali
Izod Impact, Notched 2.26 J/cm

@Thickness 3.20 mm
4.22 ft-lb/in

@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron KU600N ABS Heat Resistant
High ImpactInformation provided by Bhansali
Izod Impact, Notched 2.26 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.22 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical SG175G ABS, Super Surface Gloss, High Flow
Feature: Injection Molding, Super Surface Gloss, High FlowApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 2.26 J/cm

@Thickness 3.20 mm
4.22 ft-lb/in

@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron IM14GL ABS Injection Molding Grade
Super High Rigidity, Medium Impact, High Chemical ResistanceInformation provided by Bhansali
Izod Impact, Notched 2.26 J/cm

@Thickness 3.20 mm
4.22 ft-lb/in

@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron IM21G ABS Injection Molding Grade
Super High Gloss, Medium ImpactInformation provided by Bhansali