Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.25 J/cm @Thickness 3.20 mm |
4.22 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron SE-22 FR Flame Retardant ABS Grade Information provided by Bhansali |
|||
Izod Impact, Notched | 2.25 J/cm @Thickness 3.20 mm |
4.22 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron SE-22 FR Flame Retardant ABS Grade Information provided by Bhansali |