Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.20 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
5.99 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 84110 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
5.99 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding MR201 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 3.20 J/cm @Temperature -40.0 °C |
6.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Oxford Polymers 802-I Polycarbonate/Polybutylene Terephthalate (PBT) Alloy Polycarbonate/Polybutylene Terephthalate (PBT) AlloyInformation provided by Oxford Polymers. |
|||
Izod Impact, Notched | 3.20 J/cm @Temperature -40.0 °C |
6.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources TP-FR-IM2-[color]-6 Polybutylene Terephthalate, Low Temperature Impact Modified, Flame Retardant Polybutylene Terephthalate, Low Temperature Impact Modified, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.20 mm, Temperature -10.0 °C |
5.99 ft-lb/in @Thickness 0.126 in, Temperature 14.0 °F |
ASTM D256 |
Kingfa JH960 HT10 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platingDrop down resistanc.. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
5.99 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
Kingfa PC-S809 Modified PC Features:Good mechanical propertiesSuper high impact strengthGood weather resistanceHigh glossGood processing propertiesStress cracking propertiesApplications:OA and IT partsAutomobile accessoriesEl.. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
6.00 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Lucent Polymers PC/ABS-1003 Polycarbonate+ABS, Extrusion / General Purpose, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
6.00 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Lucent Polymers PC/ABS-1211P Polycarbonate+ABS, Impact Modified, Platable, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
6.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 IM 7040 MB Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier, Nucleating Agent and LubricantFeatures: Heat Stabilized, Impact Modified, Nucleated and LubricatedInformation pro.. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
6.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 IM 7050 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier, Nucleating Agent and LubricantFeatures: Heat Stabilized, Impact Modified, Nucleated and LubricatedInformation pro.. |
|||
Izod Impact, Notched | 3.20 J/cm @Temperature -40.0 °C |
5.99 ft-lb/in @Temperature -40.0 °F |
Practical Use (Water Absorption 2.0%); ASTM-D256 |
Toyobo GLAMIDE® T-222SA Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |