Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.01 J/cm @Thickness 3.18 mm, Temperature -20.0 °C |
1.89 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-115GF-AX00 PC+PBT with Glass Fiber Reinforcement
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar GN002 Copolyester, Natural
(discontinued **) Eastar GN002 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN002 copolyester will not crystallize and thus offers wider processing latitude tha.. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar GN005 Copolyester, Natural
(discontinued **) Eastar GN005 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN005 copolyester will not crystallize and thus offers wider processing latitude tha.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.89 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa HR-528 Modified ABS Features:UL94 HB @ 1.5-3.2mmExcellent heat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd... |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Drystar 0113 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Drystar 0601 Copolyester, Injection Molded This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar MN210 Copolyester, Natural Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates.Applications/UsesMedical |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar MN211 Copolyester, Natural Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. MN211 contains a mold release.Application.. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastman 1223 Copolyester Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card.. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman GSP01 Copolyester for Film and Sheet Extrusion Applications:Consumer e-packaging trayElectronic packagingElectrostatic dissipative trayProduct Description: GSP01 is a clear, amorphous material. Because of its clarity, toughness and good melt s.. |