Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.780 J/cm @Thickness 3.17 mm |
1.46 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LG Chemical MI-770 MIPS |
|||
Izod Impact, Notched | 0.780 J/cm @Thickness 6.35 mm |
1.46 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
LG Chemical 40 AF Flame Retardant HIPS High impact, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, Applications include televisions, VT.. |
|||
Izod Impact, Notched | 0.780 J/cm @Thickness 6.35 mm |
1.46 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
LG Chemical 501S-S HIPS Self lubricant, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include refrigerator food holders, par.. |
|||
Izod Impact, Notched | 0.780 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.46 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® X9102 Modified Polyphenylene Ether High-Heat ResistantInformation provided by Asahi Kasei |