Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.460 J/cm @Temperature -40.0 °C |
0.862 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar GN119 Copolyester Applications:Personal care and CosmeticsProduct Description: Eastar GN119 Copolyester is a low-I.V. PETG, for sale only in Asia as a high-flow formulation. This product has been GREENGUARD INDOOR .. |
|||
Izod Impact, Notched | 0.460 J/cm @Temperature -40.0 °C |
0.862 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar GN120 Copolyester Applications:AppliancesConsumer electronicsPersonal care and cosmeticsStationary suppliesKey Attributes:High clarity and transparencyHigh flow copolyesterToughProduct Description: Eastar GN120 Cop.. |