Mechanical Properties Metric English Comments
Izod Impact, Notched 0.460 J/cm

@Temperature -40.0 °C
0.862 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman Eastar GN119 Copolyester
Applications:Personal care and CosmeticsProduct Description: Eastar GN119 Copolyester is a low-I.V. PETG, for sale only in Asia as a high-flow formulation. This product has been GREENGUARD INDOOR ..
Izod Impact, Notched 0.460 J/cm

@Temperature -40.0 °C
0.862 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman Eastar GN120 Copolyester
Applications:AppliancesConsumer electronicsPersonal care and cosmeticsStationary suppliesKey Attributes:High clarity and transparencyHigh flow copolyesterToughProduct Description: Eastar GN120 Cop..