Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.352 J/cm @Temperature -17.8 °C |
0.660 ft-lb/in @Temperature 0.000 °F |
ASTM D256A |
ExxonMobil AP3AW Polypropylene Impact Copolymer Product Description: A UV stabilized medium impact copolymer resin designed for automotive battery cases.Availability: Asia Pacific Features:Good UV ResistanceHigh StiffnessLow WarpageMedium FlowMe.. |