Mechanical Properties Metric English Comments
Izod Impact, Notched 0.352 J/cm

@Temperature -17.8 °C
0.660 ft-lb/in

@Temperature 0.000 °F
ASTM D256A
ExxonMobil AP3AW Polypropylene Impact Copolymer
Product Description: A UV stabilized medium impact copolymer resin designed for automotive battery cases.Availability: Asia Pacific Features:Good UV ResistanceHigh StiffnessLow WarpageMedium FlowMe..