Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.540 J/cm @Temperature 23.0 °C |
1.01 ft-lb/in @Temperature 73.4 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® NB-5620S Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.540 J/cm @Temperature -40.0 °C |
1.01 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® TY-145TZ Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.540 J/cm @Temperature 23.0 °C |
1.01 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Toyobo NB-5620S Nylon/Olefin Alloy, 15% Mineral Reinforced (DAM) Features: 15% Mineral Reinforced, Light WeightInformation provided by Toyobo. |
|||
Izod Impact, Notched | 0.540 J/cm @Temperature 23.0 °C |
1.01 ft-lb/in @Temperature 73.4 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-802 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.540 J/cm @Temperature 23.0 °C |
1.01 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar EN010 Copolyester Eastar copolyester EN010 is used primarily in molded thick wall European applications.Applications/UsesPackagingInjection moldingContainers |
|||
Izod Impact, Notched | >= 0.540 J/cm @Temperature 0.000 °C |
>= 1.01 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
Eastman TiGlaze SV Copolyester TiGLAZE SV copolyester is a specialty copolyester for the architectural glazing industry, designed to provide a unique balance of toughness, stiffness and material value. The material has a CC1 Ligh.. |