Mechanical Properties Metric English Comments
Impact Test 9.90 - 18.0 J
7.30 - 13.3 ft-lb
Instrumented Impact Total Energy; ASTM D3763
ExxonMobil LD 503.LN Foams and Compounding Resin  (discontinued **)
LD 503.LN is a low density homopolymer specially designed for maximum performance in foam applications.Information provided by ExxonMobil Chemical