Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 9.90 - 18.0 J | 7.30 - 13.3 ft-lb | Instrumented Impact Total Energy; ASTM D3763 |
ExxonMobil LD 503.LN Foams and Compounding Resin
(discontinued **) LD 503.LN is a low density homopolymer specially designed for maximum performance in foam applications.Information provided by ExxonMobil Chemical |