Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 103 J | 76.0 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics Geloy XTPM309E ASA+PC (Europe-Africa-Middle East) XTPM309E is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour stab.. |
|||
Impact Test | 103 J | 76.0 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON DEI13F PC (Asia Pacific) LNP* Stat-kon* DEI13F is a compound based on Polycarbonate resin containing Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Superior Molding, Internally Lu.. |
|||
Impact Test | 103 J | 76.0 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON DEI13F PC LNP* STAT-KON* DEI13F is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 2% Silicone. Added features of this material include: Electrically Conductive, Superior Molding, Wear R.. |
|||
Impact Test | 103 J | 76.0 ft-lb | ASTM D3763 |
Braskem TI60035NB High Impact Copolymer Polypropylene Description: Extra high izod impact, superior low temperature drop impact.Applications: Suggested uses include compounding, automotive, injection molding.Process: Injection Molding. This resin meets.. |