Material Notes:
Description: Extra high izod impact, superior low temperature drop impact.Applications: Suggested uses include compounding, automotive, injection molding.Process: Injection Molding. This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 3.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 76
76
ASTM D785
Tensile Strength 21.4 MPa
3100 psi
2 in/min; ASTM D638
Elongation at Yield 9.0 %
9.0 %
2 in/min; ASTM D638
Flexural Modulus 0.965 GPa
140 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched NB
NB
ASTM D256A
Impact Test 103 J
76.0 ft-lb
ASTM D3763