Impact Test 103 J
76.0 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Geloy XTPM309E ASA+PC (Europe-Africa-Middle East)
XTPM309E is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour stab..
Impact Test 103 J
76.0 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-KON DEI13F PC (Asia Pacific)
LNP* Stat-kon* DEI13F is a compound based on Polycarbonate resin containing Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Superior Molding, Internally Lu..
Impact Test 103 J
76.0 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-KON DEI13F PC
LNP* STAT-KON* DEI13F is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 2% Silicone. Added features of this material include: Electrically Conductive, Superior Molding, Wear R..
Impact Test 103 J
76.0 ft-lb
ASTM D3763
Braskem TI60035NB High Impact Copolymer Polypropylene
Description: Extra high izod impact, superior low temperature drop impact.Applications: Suggested uses include compounding, automotive, injection molding.Process: Injection Molding. This resin meets..