Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.02099 GPa | 3.045 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials PEARLTHANE® 11T92E Thermoplastic Polyurethane Elastomer Type: Pearlthane® 11T92E is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining hardness with excellent mechanical pr.. |
|||
300% Modulus | 0.02099 GPa | 3.045 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Black Peroxide Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
300% Modulus | 0.02099 GPa | 3.045 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR Di-Cup 40C Peroxide, Hardness 65A Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
300% Modulus | 0.02099 GPa | 3.045 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR Di-Cup 40C Peroxide, Hardness 65A Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
300% Modulus | 0.02099 GPa | 3.045 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Black Peroxide Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |