Mechanical Properties Metric English Comments
300% Modulus 0.02099 GPa
3.045 ksi
ISO 527-2/5A/500
Lubrizol Advanced Materials PEARLTHANE® 11T92E Thermoplastic Polyurethane Elastomer
Type: Pearlthane® 11T92E is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining hardness with excellent mechanical pr..
300% Modulus 0.02099 GPa
3.045 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Black Peroxide Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
300% Modulus 0.02099 GPa
3.045 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR Di-Cup 40C Peroxide, Hardness 65A
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
300% Modulus 0.02099 GPa
3.045 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR Di-Cup 40C Peroxide, Hardness 65A
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
300% Modulus 0.02099 GPa
3.045 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Black Peroxide Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..