Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00483 GPa | 0.701 ksi | ASTM D412 |
Kraton® G1652 E (SEBS) Linear Block Copolymer Description: Kraton G1652 E polymer is a clear, linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 30% mass. It is supplied from Europe in the physical .. |
|||
300% Modulus | 0.00483 GPa | 0.701 ksi | ASTM D412 |
Kraton® G1652 H (SEBS) Linear Triblock Copolymer Description: Kraton G1652 H is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form ide.. |
|||
300% Modulus | 0.00483 GPa | 0.701 ksi | ASTM D412 |
Kraton® G1652 M (SEBS) Linear Triblock Copolymer Description: Kraton G1652 M is a translucent, linear triblock copolymer based on styrene and ethylene/butylene (SEBS) with a Styrene / Rubber ratio of 30/70. It is supplied from North America in the.. |