Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00483 GPa | 0.701 ksi | ASTM D412 |
Kraton® G1652 E (SEBS) Linear Block Copolymer Description: Kraton G1652 E polymer is a clear, linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 30% mass. It is supplied from Europe in the physical .. |
|||
300% Modulus | 0.00483 GPa | 0.701 ksi | ASTM D412 |
Kraton® G1652 H (SEBS) Linear Triblock Copolymer Description: Kraton G1652 H is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form ide.. |
|||
300% Modulus | 0.00483 GPa | 0.701 ksi | ASTM D412 |
Kraton® G1652 M (SEBS) Linear Triblock Copolymer Description: Kraton G1652 M is a translucent, linear triblock copolymer based on styrene and ethylene/butylene (SEBS) with a Styrene / Rubber ratio of 30/70. It is supplied from North America in the.. |
|||
300% Modulus | 0.00483 GPa | 0.700 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00483 - 0.00965 GPa | 0.700 - 1.40 ksi | Secant; Conditioned 7 days at RT/50% RH; ASTM D638 |
AdvanSource Biomaterials ChronoFlex® C 80A Biodurable Medical Grade Polyurethane ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome.. |
|||
300% Modulus | 0.00483 GPa | 0.700 ksi | ASTM D412-75 |
3M SJ-1FB Cold Shrink Foldback Splice Jacket Kits 3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice.. |
|||
300% Modulus | 0.00483 GPa | 0.700 ksi | ASTM D412-75 |
3M SJ-2FB Cold Shrink Foldback Splice Jacket Kits 3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice.. |
|||
300% Modulus | 0.00483 GPa | 0.700 ksi | ASTM D412-75 |
3M SJ-3FB Cold Shrink Foldback Splice Jacket Kits 3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice.. |
|||
300% Modulus | 0.00483 GPa | 0.700 ksi | ASTM D412-75 |
3M SJ-4FB Cold Shrink Foldback Splice Jacket Kits 3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice.. |
|||
300% Modulus | 0.00483 GPa | 0.700 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |