Kraton® G1652 M (SEBS) Linear Triblock Copolymer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Kraton
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® G1652 M (SEBS) Linear Triblock Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Kraton G1652 M is a translucent, linear triblock copolymer based on styrene and ethylene/butylene (SEBS) with a Styrene / Rubber ratio of 30/70. It is supplied from North America in the physical form identified: Kraton G1652 MU - supplied as an undusted powderKraton G1652 MS - supplied as a dusted powderRegion: Asia Pacific, Europe, Japan, North America, and South AmericaUses: Kraton G1652 M is used as a modifier of bitumen and polymers. It is also suitable as an ingredient in formulating compounds for footwear applications and may be used in formulating adhesives, sealants, and coatings.Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Bitumen ModificationInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D4025
Volatiles <= 0.60 %
<= 0.60 %
KM 04
Viscosity 400 - 525 cP
400 - 525 cP
20% Toluene Solution at 25°C; BAM 922
Melt Flow 5.0 g/10 min

@Load 5.00 kg,
Temperature 230 °C
5.0 g/10 min

@Load 11.0 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 69

@Time 10.0 sec
69

@Time 0.00278 hour
ASTM D2240
Tensile Strength 31.0 MPa
4500 psi
ASTM D412
Elongation at Break 500 %
500 %
ASTM D412
300% Modulus 0.00483 GPa
0.701 ksi
ASTM D412
Descriptive Properties Value Comments
Content Non-staining phenolic antioxidant
0.03-0.1%, KM 08
Polystyrene
29-30.8%, Measured on the polymer before hydrogenation, KM 03
Total Extractables
<1.0%, KM 05
Styrene/Rubber Ratio 30/70