Polymer Property : 300% Modulus = 0.0164 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.0164 GPa
2.38 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 6.0 PHR MBTS
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
300% Modulus 0.0164 GPa
2.38 ksi
DIN 53504
Lubrizol ESTANE® 5701F1 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
300% Modulus 0.0164 GPa
2.38 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 6.0 PHR MBTS
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
300% Modulus 0.0164 - 0.0203 GPa
2.38 - 2.94 ksi
35 min cured; ASTM D412
Iran Petrochemical (PCC) SBR-1502 Styrene Butadiene Rubber
SBR–1502 is a cold, 23.5% styrene SBR polymer made with a mixed-acid emulsifier, a non-staining stabilizer and a salt–acid coagulation. Provided that the compounds are formulated and processed cor..