TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 6.0 PHR MBTS

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 6.0 PHR MBTS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.The combination of thiazole accelerators, MBTS and MBT, enable the best possible cure for Millathane® 76. An increase in MBTS results in a higher state of cure and increased processing safety.An increase in MBT decreases scorch time and increases the state of cure.All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 69
69
Tensile Strength, Yield 32.0 MPa
4640 psi
Elongation at Yield 515 %
515 %
100% Modulus 0.00403 GPa
0.585 ksi
200% Modulus 0.009480 GPa
1.375 ksi
300% Modulus 0.0164 GPa
2.38 ksi
Tear Strength 61.3 kN/m
350 pli
Die C
Compression Set 29.7 %

@Temperature 70.0 °C,
Time 79200 sec
29.7 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 4.40 min

@Temperature 155 °C
0.0733 hour

@Temperature 311 °F
ts2
10.8 min

@Temperature 155 °C
0.180 hour

@Temperature 311 °F
TC90