Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) SBR-1502 Styrene Butadiene Rubber

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) SBR-1502 Styrene Butadiene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SBR–1502 is a cold, 23.5% styrene SBR polymer made with a mixed-acid emulsifier, a non-staining stabilizer and a salt–acid coagulation. Provided that the compounds are formulated and processed correctly, the vulcanizates have very good abrasion , good heat and aging resistance, good mechanical properties , good electrical properties and good resistance to polar solvents and dilute acids. Applications: end uses include white sidewall tyres, foot wear, light and dark coloured mechanical goods and miscellaneous items where excellent physical properties and minimum discoloration and staining are required.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Volatiles <= 0.75 %
<= 0.75 %
ASTM D1416
Viscosity Measurement 46 - 58
46 - 58
raw viscosity, ML 1+4 @ 100°C; ASTM D1646
<= 84
<= 84
compound viscosity, ML 1+4 @ 100°C; ASTM D1646
Ash <= 1.5 %
<= 1.5 %
ASTM D1416
Mechanical Properties Metric English Comments
Tensile Strength >= 24.5 MPa
>= 3560 psi
35 min cured; ASTM D412
Elongation at Break 350 %
350 %
35 min cured; ASTM D412
300% Modulus 0.0164 - 0.0203 GPa
2.38 - 2.94 ksi
35 min cured; ASTM D412
Chemical Properties Metric English Comments
Styrene Content 23 %
23 %
ASTM D1416
Descriptive Properties Value Comments
Organic Acid, % 5.875
ASTM D1416
Soap, % < 0.5
ASTM D1416
Users viewing this material also viewed the following: