Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00827 GPa | 1.20 ksi | 25 mil film; ASTM D412 |
Huntsman IROGRAN® A 85 P 4394 UV TPU-Polyether Introduction: IROGRAN A 85 P 4394 is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4394 is part of the HUNTS.. |
|||
300% Modulus | 0.00827 GPa | 1.20 ksi | 25 mil film; ASTM D412 |
Huntsman IROGRAN® A 85 P 5004 TPU-Polyether IROGRAN® A 85 P 5004 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications.Information provided by Alliance Polymers |
|||
300% Modulus | 0.00827 GPa | 1.20 ksi | ASTM D412 |
Huntsman KRYSTALFLEX® PE 429 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
300% Modulus | 0.00827 GPa | 1.20 ksi | ASTM D412-92 |
Saint-Gobain Tygothane® C-544-AI.B. Precision Polyurethane Pressure Tubing Formulation Description: Tygothane® C-544-A I.B.: More flexible than many other reinforced urethane tubings, Tygothane® Pressure Tubing can be used in some of the most physically demanding applications,.. |
|||
300% Modulus | 0.00827 GPa | 1.20 ksi | ASTM D412 |
Lubrizol Estane® AG 4350 Thermoplastic Polyurethane Type: Estane® AG 4350 is a polyether based aliphatic polyurethane specifically formulated to be used as an adhesive interlayer without the need for a glass surface primer. This polymer is designed.. |
|||
300% Modulus | 0.00827 GPa | 1.20 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.00827 GPa | 1.20 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |