Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is carried out by the use of various peroxides including dicumyl peroxide (DCP) or 2,5-dimethyl-2,5-bis (t-butylperoxy) hexane (DBPH).FormulationMillathane 5004100Stearic Acid0.25Hi-Sil 23340Di-Cup 40C8All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
Tensile Strength, Yield 22.1 MPa
3200 psi
Elongation at Yield 540 %
540 %
100% Modulus 0.00276 GPa
0.400 ksi
200% Modulus 0.00503 GPa
0.730 ksi
300% Modulus 0.00758 GPa
1.10 ksi
Tear Strength 63.0 kN/m
359 pli
ASTM Die C
Processing Properties Metric English Comments
Cure Time 2.00 min

@Temperature 204 °C
0.0333 hour

@Temperature 400 °F
Users viewing this material also viewed the following: