Saint-Gobain Tygothane® C-544-AI.B. Precision Polyurethane Pressure Tubing Formulation

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Tygothane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Tygothane® C-544-AI.B. Precision Polyurethane Pressure Tubing Formulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Tygothane® C-544-A I.B.: More flexible than many other reinforced urethane tubings, Tygothane® Pressure Tubing can be used in some of the most physically demanding applications, such as those requiring a tight bend radius. Specially formulated from tough, ether-based polyurethane resin, Tygothane® Pressure Tubing is resistant to a range of chemicals, including oils, greases, solvents and chemicals. Because of its excellent wear properties, Tygothane® Pressure Tubing frequently outperforms traditional rubber, plastic and metal materials when exposed to abrasive conditions. Tygothane® Pressure Tubing is also plasticizer free, and remains flexible even when cycled through temperature extremes.Features/Benefits:Exceptional abrasion and tear resistanceTough braid reinforcement for elevated working pressuresExcellent resistance to oils, greases and fuelsRetains flexibility in sub-zero environmentsIdeal for use with Tygopure™ reusable fittingsMeets FDA and NSF 51 criteria for food contactMeets NSF 61 criteria for potable water contactTypical applications include Food and Cosmetic Processing, Abrasive and Viscous Slurry Transfer, Lubrication and Degreaser Dispensing, pellet and Powder Transfer, Pneumatic Sensory Devices, Instrumentation Control Lines, Coolant Recovery Systems.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792-91
Water Absorption 1.8 %
1.8 %
24 hours at 23°C; ASTM D570-81
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
15 seconds; ASTM D2240-91
Tensile Strength, Yield 34.5 MPa
5000 psi
ASTM D412-92
Elongation at Break 400 %
400 %
ASTM D412-92
100% Modulus 0.00552 GPa
0.800 ksi
ASTM D412-92
300% Modulus 0.00827 GPa
1.20 ksi
ASTM D412-92
Tear Strength 61.4 kN/m
350 pli
Initial Tear Strength; ASTM D1004-93
Compression Set 19 %

@Temperature 70.0 °C
19 %

@Temperature 158 °F
Constant Deflection, for 22 hrs.; ASTM D395-89 Method B
Tensile Set 45 %
45 %
ASTM D412-92
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.2 °C
180 °F
Brittleness Temperature -73.3 °C
-100 °F
ASTM D746-79
Electrical Properties Metric English Comments
Dielectric Strength 21.7 kV/mm
550 kV/in
ASTM D149-93
Descriptive Properties Value Comments
Color Clear