Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 3.86 MPa | 560 psi | NBR-NBR; Substrate Failure; Tensile Lap Shear |
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver.. |
|||
Adhesive Bond Strength | 3.86 MPa | 560 psi | Neoprene-Neoprene; Substrate Failure; Tensile Lap Shear |
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver.. |
|||
Adhesive Bond Strength | >= 3.86 MPa | >= 560 psi | Excellent - 100% Concrete Failure |
Chesterton ARC NVE SYSTEM Vinyl Ester Lining Description: ARC NVE is a high performance, quartz reinforced, three-component, modified novolac vinyl ester lining capable of being applied to horizontal and vertical surfaces. The NVE system kit i.. |
|||
Adhesive Bond Strength | >= 3.86 MPa | >= 560 psi | Wet concrete; ASTM D4541 |
Chesterton ARC CS2 Low-viscosity, Composite concrete primer sealer Description: An advanced composite formulated to protect concrete surfaces from mild chemical attack. It is normally applied at a thickness of 250-375 microns (10-15 mils) per coat. Non-shrinking. 1.. |