Mechanical Properties Metric English Comments
Adhesive Bond Strength 3.86 MPa
560 psi
NBR-NBR; Substrate Failure; Tensile Lap Shear
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate
Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver..
Adhesive Bond Strength 3.86 MPa
560 psi
Neoprene-Neoprene; Substrate Failure; Tensile Lap Shear
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate
Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver..
Adhesive Bond Strength >= 3.86 MPa
>= 560 psi
Excellent - 100% Concrete Failure
Chesterton ARC NVE SYSTEM Vinyl Ester Lining
Description: ARC NVE is a high performance, quartz reinforced, three-component, modified novolac vinyl ester lining capable of being applied to horizontal and vertical surfaces. The NVE system kit i..
Adhesive Bond Strength >= 3.86 MPa
>= 560 psi
Wet concrete; ASTM D4541
Chesterton ARC CS2 Low-viscosity, Composite concrete primer sealer
Description: An advanced composite formulated to protect concrete surfaces from mild chemical attack. It is normally applied at a thickness of 250-375 microns (10-15 mils) per coat. Non-shrinking. 1..