Adhesive Bond Strength 19.0 - 23.0 MPa
2760 - 3340 psi
Steel, Shear; ISO 4587
Permabond 101 Cyanoacrylate, Wicking Viscosity
PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya..
Adhesive Bond Strength 19.0 - 23.0 MPa
2760 - 3340 psi
Steel, Shear; ISO 4587
Permabond 2010 Cyanoacrylate, gap filling
PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy..
Adhesive Bond Strength 19.0 - 23.0 MPa
2760 - 3340 psi
Steel, Shear; ISO 4587
Permabond 737 Cyanoacrylate, toughened
PERMABOND® 737 is a toughened cyanoacrylate with improved impact and peel strength for maximum flexibility. Its increased temperature resistance and dark color make 737 suitable for a wide range of..
Adhesive Bond Strength 19.0 - 23.0 MPa
2760 - 3340 psi
Steel, Shear; ISO 4587
Permabond 922 Cyanoacrylate, High temperature
PERMABOND® 922 is the original allyl cyanoacrylate adhesive. It is a single part, moderate viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. P..
Adhesive Bond Strength 19.0 - 23.0 MPa
2760 - 3340 psi
FRP Glass Epoxy, Shear; ISO 4587
Permabond ET5401 Epoxy Resin
PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo..
Adhesive Bond Strength 19.0 - 23.0 MPa
2760 - 3340 psi
Steel, Shear; ISO 4587
Permabond 102 Cyanoacrylate, General purpose
PERMABOND® 102 is a low viscosity general purpose cyanoacrylate adhesive suitable for bonding close-fitting components. It is fast setting and suitable for use on plastics, rubber and metals. Cyano..
Adhesive Bond Strength 19.0 - 23.0 MPa
2760 - 3340 psi
ISO 4587, Shear
Permabond 801 Cyanoacrylate, High Temperature
PERMABOND® 801 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber..
Adhesive Bond Strength 19.0 - 23.0 MPa
2760 - 3340 psi
ISO 4587, Shear
Permabond 802 Cyanoacrylate, High Temperature
PERMABOND® 802 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber..
Adhesive Bond Strength 19.0 - 23.0 MPa
2760 - 3340 psi
ISO 4587, Shear
Permabond 820 Cyanoacrylate, High Temperature
PERMABOND® 820 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber..
Adhesive Bond Strength 19.0 - 23.0 MPa
2760 - 3340 psi
Steel, Shear; ISO 4587
Permabond 920 Cyanoacrylate, High temperature
PERMABOND® 920 is the original allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMAB..