Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 19.0 - 23.0 MPa | 2760 - 3340 psi | Steel, Shear; ISO 4587 |
Permabond 101 Cyanoacrylate, Wicking Viscosity PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya.. |
|||
Adhesive Bond Strength | 19.0 - 23.0 MPa | 2760 - 3340 psi | Steel, Shear; ISO 4587 |
Permabond 2010 Cyanoacrylate, gap filling PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy.. |
|||
Adhesive Bond Strength | 19.0 - 23.0 MPa | 2760 - 3340 psi | Steel, Shear; ISO 4587 |
Permabond 737 Cyanoacrylate, toughened PERMABOND® 737 is a toughened cyanoacrylate with improved impact and peel strength for maximum flexibility. Its increased temperature resistance and dark color make 737 suitable for a wide range of.. |
|||
Adhesive Bond Strength | 19.0 - 23.0 MPa | 2760 - 3340 psi | Steel, Shear; ISO 4587 |
Permabond 922 Cyanoacrylate, High temperature PERMABOND® 922 is the original allyl cyanoacrylate adhesive. It is a single part, moderate viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. P.. |
|||
Adhesive Bond Strength | 19.0 - 23.0 MPa | 2760 - 3340 psi | FRP Glass Epoxy, Shear; ISO 4587 |
Permabond ET5401 Epoxy Resin PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo.. |
|||
Adhesive Bond Strength | 19.0 - 23.0 MPa | 2760 - 3340 psi | Steel, Shear; ISO 4587 |
Permabond 102 Cyanoacrylate, General purpose PERMABOND® 102 is a low viscosity general purpose cyanoacrylate adhesive suitable for bonding close-fitting components. It is fast setting and suitable for use on plastics, rubber and metals. Cyano.. |
|||
Adhesive Bond Strength | 19.0 - 23.0 MPa | 2760 - 3340 psi | ISO 4587, Shear |
Permabond 801 Cyanoacrylate, High Temperature PERMABOND® 801 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber.. |
|||
Adhesive Bond Strength | 19.0 - 23.0 MPa | 2760 - 3340 psi | ISO 4587, Shear |
Permabond 802 Cyanoacrylate, High Temperature PERMABOND® 802 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber.. |
|||
Adhesive Bond Strength | 19.0 - 23.0 MPa | 2760 - 3340 psi | ISO 4587, Shear |
Permabond 820 Cyanoacrylate, High Temperature PERMABOND® 820 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber.. |
|||
Adhesive Bond Strength | 19.0 - 23.0 MPa | 2760 - 3340 psi | Steel, Shear; ISO 4587 |
Permabond 920 Cyanoacrylate, High temperature PERMABOND® 920 is the original allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMAB.. |