Trelleborg Emerson & Cuming Eccobond® 45 Two-Component General Purpose Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Eccobond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Eccobond® 45 Two-Component General Purpose Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Emerson & Cuming 45 Eccobond® Two-Component General Purpose Epoxy AdhesiveFilled, general purpose, room temperature curing, epoxy adhesive and sealant. Flexibility can be adjusted by the amount of Catalyst 15 used. Convenient mix ratio. Good impact resistance. Excellent adhesion to metal, glass and plastic substrates. Mix Ratio of 100:50 to 100:150 (Cat 15 variation). Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 1.18 - 1.34 g/cc
0.0426 - 0.0484 lb/in³
Viscosity 37000 cP

@Temperature 25.0 °C
37000 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Adhesive Bond Strength 21.4 MPa
3100 psi
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature >=105 °C
0.250 hour

@Temperature >=221 °F
30.0 min

@Temperature 70.0 °C
0.500 hour

@Temperature 158 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Black