Adhesive Bond Strength 30.0 MPa
4350 psi
steel collar and pin shear; ISO 10123
Permabond F202 Anaerobic Retainer
The unique 'toughening' process incorporated into Permabond® F202 gives this anaerobic adhesive excellent resistance to peel and impact forces. Primarily designed for use on metal surfaces, it is a..
Adhesive Bond Strength 30.0 MPa
4350 psi
steel collar and pin shear; ISO 10123
Permabond HM162 Anaerobic Retainer
Permabond® HM162 is a medium viscosity retaining compound that cures when confined between metal parts to form an extremely tough bond. It is best suited for cylindrical parts and where high temper..
Adhesive Bond Strength 30.0 MPa
4350 psi
steel collar and pin shear; ISO 10123
Permabond F201 Anaerobic Retainer
Permabond® F201 is an anaerobic adhesive which has been developed to give excellent resistance to peel and impact forces. This toughening, combined with good adhesion to aluminum and copper alloys,..
Adhesive Bond Strength 30.0 MPa
4350 psi
Lap shear, alum to alum, 30 min @ 150°C
Tra-Con Tra-Bond 789-3T3N1 Moisture Resistant Adhesive
TRA-BOND 789-3T3N1 adhesive is a thixotropic version of TRA-BOND 789-3. It is a one component, high strength, toughened adhesive designed for use in applications which require good moisture resistan..
Adhesive Bond Strength 30.0 MPa

@Thickness 2.00 mm
4350 psi

@Thickness 0.0787 in
Lap Shear (25 x 10 x 0.2 mm) (CRS St 1203, 170°C/30); EN 1465
Dow BETAMATE™ 1496 V Epoxy
BETAMATE™ 1496 V is a one component, epoxy based adhesive especially developed for the body shop. The product has the following properties: Good rheology performance (Wash-out resistant, excelle..
Adhesive Bond Strength 30.0 MPa
4350 psi
Steel-Steel; after optimum cure
Armstrong C-4/D Epoxy Adhesive
A low viscosity, clear amber, unfilled adhesive, recommended for use with activators D or W. C-4 with Activator W offers maximum versatility in that differing degrees of flexibility can be achieved ..
Adhesive Bond Strength 30.0 MPa
4350 psi
steel collar and pin shear; ISO 10123
Permabond HM135 Anaerobic Retainer
Permabond® HM135 is a fast curing, medium viscosity anaerobic adhesive for locking and sealing threads and retaining cylindrical components. It gives maximum torque strength on brass or plated bras..