Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Permabond F201 Anaerobic Retainer

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Permabond
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond F201 Anaerobic Retainer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Permabond® F201 is an anaerobic adhesive which has been developed to give excellent resistance to peel and impact forces. This toughening, combined with good adhesion to aluminum and copper alloys, makes it the first choice where relatively thin or lightweight components are being bonded which may be subject to “distortion” in service. It is also capable of resisting the thermal stresses that may be generated when bonding dissimilar surfaces. Permabond F201 is also suitable for contact with potable water. Features & Benefits: Toughened Very high strength Ideal when bonding dissimilar materials Improved fatigue lifeWRAS listed for contact with potable waterInformation provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
Uncured
Viscosity 2500 cP

@Temperature 25.0 °C
2500 cP

@Temperature 77.0 °F
at 20 rpm vibration
9000 cP

@Temperature 25.0 °C
9000 cP

@Temperature 77.0 °F
at 2 rpm vibration
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Adhesive Bond Strength 30.0 MPa
4350 psi
steel collar and pin shear; ISO 10123
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Dielectric Strength 11.0 kV/mm
279 kV/in
Processing Properties Metric English Comments
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
15.0 min

@Temperature 23.0 °C
0.250 hour

@Temperature 73.4 °F
M10 steel, handling strength
30.0 min

@Temperature 23.0 °C
0.500 hour

@Temperature 73.4 °F
Brass, working strength
60.0 min

@Temperature 23.0 °C
1.00 hour

@Temperature 73.4 °F
Zinc, handling strength
60.0 min

@Temperature 23.0 °C
1.00 hour

@Temperature 73.4 °F
M10 steel, working strength
360 min

@Temperature 23.0 °C
6.00 hour

@Temperature 73.4 °F
Stainless steel, handling strength
360 - 1440 min

@Temperature 23.0 °C
6.00 - 24.0 hour

@Temperature 73.4 °F
Zinc, working strength
1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
M10 steel, full strength
Descriptive Properties Value Comments
Appearance Brown
Uncured
Maximum Gap Fill (mm) 0.5
Maximum Thread Size M20
Strength Retention 15% at 150°C
Relative to 0°C
35% at 100°C
Relative to 0°C
85% at 50°C
Relative to 0°C
Torque Strength (N m) 28
M10 steel, break
30
M10 steel, prevail
UV Fluorescence No
Uncured
Users viewing this material also viewed the following: