Material Notes:
ApplicationsLaunder linings Lining of distribution launders for DC casting table Industrial furnace linings Back up material behind hot face lining AdvantagesLow density with high insulating properties Non-wetting to molten aluminum Easy to handle Saves drying time Immediate heating for drying is possible just after molding Information provided by Pyrotek.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 1.96 - 2.94 MPa
284 - 426 psi
Transverse
Thermal Properties Metric English Comments
Thermal Conductivity 0.116 W/m-K

@Temperature 500 °C
0.805 BTU-in/hr-ft²-°F

@Temperature 932 °F
Maximum Service Temperature, Air 1300 °C
2370 °F
Shrinkage 0.600 - 0.800 %

@Temperature 800 °C,
Time 3600 sec
0.600 - 0.800 %

@Temperature 1470 °F,
Time 1.00 hour
Component Elements Properties Metric English Comments
Al2O3 24 %
24 %
SiO2 73 %
73 %