Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 21.0 MPa | 3050 psi | Brass, Shear; ISO 4587 |
Permabond 2011 Cyanoacrylate, gel PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and.. |
|||
Adhesive Bond Strength | 21.0 MPa | 3050 psi | Stainless Steel, Shear; ISO 4587 |
Permabond 2011 Cyanoacrylate, gel PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and.. |
|||
Adhesive Bond Strength | 21.0 MPa | 3050 psi | Grit-blasted Steel, Shear |
Permabond 738 Cyanoacrylate, toughened PERMABOND 738 is a toughened cyanoacrylate with improved impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable over.. |
|||
Adhesive Bond Strength | 21.0 - 25.0 MPa | 3050 - 3630 psi | Steel, Shear; ISO 4587 |
Permabond 240 Cyanoacrylate, gap filling PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate.. |
|||
Adhesive Bond Strength | 21.0 MPa | 3050 psi | Grit-blasted Steel, Shear |
Permabond 798 Cyanoacrylate, Surface insensitive PERMABOND 798 is a high viscosity cyanoacrylate that combines fast cure with the ability to cure through a large gap. Plastics, Metals, Ceramics and elastomers are also rapidly bonded. The fast cu.. |
|||
Adhesive Bond Strength | 21.0 MPa @Temperature -54.4 °C |
3050 psi @Temperature -66.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-12 Epoxy Adhesive, at 2:3 Mix Ratio Our most popular general-purpose, high viscosity adhesive for industry. Combines low toxicity with excellent physical properties, and offers a non-critical mixing ratio of 1:1 by weight. This rati.. |
|||
Adhesive Bond Strength | 21.0 MPa | 3050 psi | Steel-Steel; after optimum cure |
Armstrong C-1/A Epoxy Adhesive A versatile, low viscosity, unfilled resin used for electrical potting and laminating applications. It is an excellent insulator, and provides outstanding chemical resistance to most compoundsInfor.. |
|||
Adhesive Bond Strength | 21.0 MPa @Temperature 25.0 °C |
3050 psi @Temperature 77.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong C-7/W Epoxy Adhesive, 1:1 Mix Ratio A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may .. |
|||
Adhesive Bond Strength | 21.0 MPa @Temperature 25.0 °C |
3050 psi @Temperature 77.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong C-7/W Epoxy Adhesive, 2:3 Mix Ratio A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may .. |
|||
Adhesive Bond Strength | 21.0 MPa | 3050 psi | Brass, Shear; ISO 4587 |
Permabond 910FS Cyanoacrylate, Methyl grade PERMABOND® 910FS is the original 100%-methyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts.. |
|||
Adhesive Bond Strength | 21.0 MPa | 3050 psi | Stainless Steel, Shear; ISO 4587 |
Permabond 910FS Cyanoacrylate, Methyl grade PERMABOND® 910FS is the original 100%-methyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts.. |
|||
Adhesive Bond Strength | 21.0 MPa | 3050 psi | steel collar and pin shear; ISO 10123 |
Permabond A118 Anaerobic Retainer Permabond® A118 is an anaerobic adhesive designed to provide permanent locking and sealing of metal parts such as bearings, gears, studs and other threaded components. It exhibits high strength, ex.. |
|||
Adhesive Bond Strength | 21.0 MPa | 3050 psi | steel collar and pin shear; ISO 10123 |
Permabond A134 Anaerobic Retainer Permabond® A134 is a high-strength anaerobic product designed for the permanent locking and sealing of metal parts. Its 'non-drip' formulation makes it suitable for use on larger fittings, coarse t.. |