Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 12.0 - 14.0 MPa | 1740 - 2030 psi | Phenolic, Shear; ISO 4587 |
Permabond 101 Cyanoacrylate, Wicking Viscosity PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya.. |
|||
Adhesive Bond Strength | 12.0 - 14.0 MPa | 1740 - 2030 psi | Phenolic, Shear; ISO 4587 |
Permabond 105 Cyanoacrylate, for difficult rubbers PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives.. |
|||
Adhesive Bond Strength | 12.0 - 14.0 MPa | 1740 - 2030 psi | Mild steel, Shear |
Permabond ET500 Epoxy Resin PERMABOND ET500 is a two-part fast-setting epoxy adhesive which bonds to a wide variety of substrates such as wood, metal, ceramics and some plastics and composites. It cures rapidly at room tempera.. |
|||
Adhesive Bond Strength | 12.0 - 14.0 MPa | 1740 - 2030 psi | Phenolic, Shear |
Permabond 102 Cyanoacrylate, General purpose PERMABOND® 102 is a low viscosity general purpose cyanoacrylate adhesive suitable for bonding close-fitting components. It is fast setting and suitable for use on plastics, rubber and metals. Cyano.. |