Material Notes:
PERMABOND® ES569 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces as well as composite materials. The high bond strength of this adhesive allows it to replace mechanical fastening, soldering, brazing or welding. ES569 has been designed to be non-sagging, allowing the product to be used in large gaps and on vertical surfaces. It is also ideal for bonding electronic components as it has high wet strength and is non-stringing and produces an excellent drop profile as well as withstanding solder reflow processes. Features & Benefits: Excellent adhesive strength Excellent resistance to vibration Easy to use – no mixing required High shear and peel strength High temperature resistance Good resistance to chemicals Non-sag, thixotropic Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Uncured
Viscosity 250000 - 500000 cP

@Temperature 25.0 °C
250000 - 500000 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 2.00 - 7.00 °C
35.6 - 44.6 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Adhesive Bond Strength 9.00 - 11.0 MPa
1310 - 1600 psi
FRP Glass/Epoxy, Shear; ASTM D1002
10.0 - 12.0 MPa
1450 - 1740 psi
Carbon Fiber, Shear; ASTM D1002
14.0 - 27.0 MPa
2030 - 3920 psi
Zinc, Shear; ASTM D1002
17.0 - 31.0 MPa
2470 - 4500 psi
Aluminum, Shear; ASTM D1002
27.0 - 41.0 MPa
3920 - 5950 psi
Steel, Shear; ASTM D1002
Peel Strength 4.00 - 4.80 kN/m
22.8 - 27.4 pli
Thermal Properties Metric English Comments
CTE, linear 45.0 µm/m-°C
25.0 µin/in-°F
Thermal Conductivity 0.500 W/m-K
3.47 BTU-in/hr-ft²-°F
Processing Properties Metric English Comments
Cure Time <= 3.00 min
<= 0.0500 hour
Induction
45.0 min

@Temperature 150 °C
0.750 hour

@Temperature 302 °F
Oven
60.0 min

@Temperature 130 °C
1.00 hour

@Temperature 266 °F
Oven
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Black Paste
Uncured
Maximum Gap Fill (mm) 5
Strength Retention 100% at 0°C
Relative to 0°C
25% at 200°C
Relative to 0°C
65% at 150°C
Relative to 0°C
85% at 100°C
Relative to 0°C
95% at 50°C
Relative to 0°C
Users viewing this material also viewed the following: