Polymer Property : Adhesive Bond Strength = 11.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength >= 11.9 MPa
>= 1720 psi
Dry concrete; ASTM D4541
Chesterton ARC CS4 low-viscosity, 100% solids, barrier coating
Description: An advanced composite formulated to protect concrete surfaces from harsh chemical attack. It is normally applied at a thickness of 250-375 microns (10-15 mils) per coat in a 2 coat syst..
Adhesive Bond Strength 11.9 MPa
1720 psi
Lap Shear Strength
Epoxyset Epoxiohm EO-23M Electrically Conductive Epoxy Adhesive
EO-23M is an electrically conductive, low viscosity silver-filled epoxy adhesive. Used for hybrid / micro-electronic adhesive including die-attach and substrate attach for Rf and Microwave devices.I..