Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Epoxyset Epoxiohm EO-23M Electrically Conductive Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy, Electrically Conductive
Manufacturer Epoxyset
Trade Name Epoxiohm
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Epoxyset Epoxiohm EO-23M Electrically Conductive Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EO-23M is an electrically conductive, low viscosity silver-filled epoxy adhesive. Used for hybrid / micro-electronic adhesive including die-attach and substrate attach for Rf and Microwave devices.Information provided by Epoxyset Inc.
Physical Properties Metric English Comments
Density 3.00 g/cc
0.108 lb/in³
Viscosity 4000 - 5000 cP
4000 - 5000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
ASTM D2240
Shear Strength 24.0 MPa
3480 psi
Adhesive Bond Strength 11.9 MPa
1720 psi
Lap Shear Strength
Thermal Properties Metric English Comments
CTE, linear 49.0 µm/m-°C
27.2 µin/in-°F
Thermal Conductivity 1.80 W/m-K
12.5 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Glass Transition Temp, Tg 68.0 °C
154 °F
Electrical Properties Metric English Comments
Electrical Resistivity 0.000400 ohm-cm
0.000400 ohm-cm
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 65.0 °C
2.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 120 min
120 min
Copyright © lookpolymers.com All Rights Reserved