Material Notes:
Description: An advanced composite formulated to protect concrete surfaces from harsh chemical attack. It is normally applied at a thickness of 250-375 microns (10-15 mils) per coat in a 2 coat system. Non-shrinking. 100% solids. ARC CS4 is a low viscosity, high performance composite coating that can be easily applied by brush, notched squeegee, roller, or spray equipment. ARC CS4 yields excellent barrier properties for long-term chemical resistance in immersion exposures. The cured ARC CS4 provides a high gloss surface with adhesion to dry and wet concrete. Benefits:Resistance to a broad range of inorganic and organic acids, caustics and other chemical solutionsOutlasts conventional paints and coatingsLong pot life allows for ease of use100% solids, no shrinkage on cureOutstanding adhesion insures reliable performance Suggested Uses:Chemical TanksSecondary ContainmentChemical Plant FloorsSumps and DikesDrainage TroughsPump BasesEquipment FoundationsInformation provided by Chesterton
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Cured
Mechanical Properties Metric English Comments
Hardness, Shore D 79
79
ASTM D2240
Tensile Strength at Break 21.0 MPa
3050 psi
ASTM D638
Elongation at Break 8.0 %
8.0 %
ASTM D638
Flexural Strength 40.5 MPa
5880 psi
ASTM D790
Flexural Modulus 1.31 GPa
190 ksi
ASTM D790
Compressive Strength 94.80 MPa
13750 psi
ASTM D695
Adhesive Bond Strength >= 11.9 MPa
>= 1720 psi
Dry concrete; ASTM D4541
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 40.0 °C
104 °F
Wet Service (Continuous)
52.0 °C
126 °F
Wet Service (Intermittent)
80.0 °C
176 °F
Dry Service
Processing Properties Metric English Comments
Cure Time 360 min

@Temperature 32.0 °C
6.00 hour

@Temperature 89.6 °F
Foot Traffic
540 min

@Temperature 32.0 °C
9.00 hour

@Temperature 89.6 °F
Light Load
600 min

@Temperature 25.0 °C
10.0 hour

@Temperature 77.0 °F
Foot Traffic
720 min

@Temperature 16.0 °C
12.0 hour

@Temperature 60.8 °F
Foot Traffic
960 min

@Temperature 10.0 °C
16.0 hour

@Temperature 50.0 °F
Foot Traffic
960 min

@Temperature 25.0 °C
16.0 hour

@Temperature 77.0 °F
Light Load
1200 min

@Temperature 32.0 °C
20.0 hour

@Temperature 89.6 °F
Full Load
1440 min

@Temperature 16.0 °C
24.0 hour

@Temperature 60.8 °F
Light Load
1800 min

@Temperature 25.0 °C
30.0 hour

@Temperature 77.0 °F
Full Load
2160 min

@Temperature 10.0 °C
36.0 hour

@Temperature 50.0 °F
Light Load
2400 min

@Temperature 16.0 °C
40.0 hour

@Temperature 60.8 °F
Full Load
3840 min

@Temperature 10.0 °C
64.0 hour

@Temperature 50.0 °F
Full Load
4800 min

@Temperature 32.0 °C
80.0 hour

@Temperature 89.6 °F
Full Chemical
6000 min

@Temperature 25.0 °C
100 hour

@Temperature 77.0 °F
Full Chemical
8400 min

@Temperature 16.0 °C
140 hour

@Temperature 60.8 °F
Full Chemical
10800 min

@Temperature 10.0 °C
180 hour

@Temperature 50.0 °F
Full Chemical
Descriptive Properties Value Comments
Color Red
Thermal Compatibility to Concrete Pass
5 cycles/dry<-10°C to 50°C (<14°F to 122°F)